Tarps ain’t tarps. The performance demands on a grain cover are far greater than the average tarpaulin. Australia’s UV intensity is one reason grain covers need to be designed to much higher specification than a standard tarpaulin.

How Harsh Is Australian Sunlight?

Solar exposure is often measured in kilolangleys (kLy) per year. On world maps of kLy annual exposure, Australia sits among the most heavily exposed regions on earth. Australia receives around 180 kLy a year, double the 85 kLy of Germany, so the UV degradation of a cover in New South Wales would be expected to be double that of the same cover in Germany (Scheirs and Parry, ExcelPlas Geomembrane Testing Services). For comparison, ‘death valley’ in Nevada, USA, which has daytime temperatures that can reach 50 degrees, has a comparatively low annual cumulative radiation of 140 kLy. This demonstrates how temperature and UV intensity quite separate variables.

The ultraviolet radiation is what causes the degradation. Wavelengths between 300 and 400 nanometres are the most damaging to polymers, because they carry enough energy to break chemical bonds. In January, clear-sky UV Index readings of 11 or more, the “extreme” category, are forecast across most of the country (Australian Radiation Protection and Nuclear Safety Agency (ARPANSA) and Cancer Council, January 2026).

What UV Does to a Grain Cover

In polypropylene (PP), UV energy breaks the long polymer chains into shorter ones, a process known as chain scission. Shorter chains mean a weaker, more brittle material.

In polyvinyl chloride (PVC), UV and heat strip hydrogen chloride from the polymer, leaving behind sequences of carbon double bonds. These sequences absorb more light, which drives further degradation and which can turn the material a more yellow colour. They can also link neighbouring chains together, stiffening the coating.

PVC coatings depend on plasticiser, an additive that sits between the polymer chains and keeps the material flexible. Plasticiser is often the first additive to leave the material, migrating to the surface and evaporating under heat and UV. As it goes, the coating hardens and shrinks.

The end result is the same in both materials. The coating hardens and cracks, the cover loses its water and gas tightness, and once UV reaches the base-cloth, the yarns themselves weaken and tear strength falls. Testing laboratories commonly treat a 50 per cent loss of original tensile strength as the point of failure, by which time the surface shows a crosshatched pattern of fine cracks when flexed (Scheirs and Parry).

How a Quality Cover Resists UV

  • UV stabilisers in the coating, additives that absorb UV or neutralise the chemical reactions it starts, before they reach the polymer chains.
  • UV stabilisers in the base-cloth, so the yarns are protected too, and are not left defenceless if the coating is scuffed or cracked.
  • Coating thickness, a thicker coating is a mechanical barrier. Degradation starts at the surface, and more material means more of it must be lost before UV reaches the base-cloth.
  • The right raw materials, the brand and grade of resin, plasticiser and UV stabiliser all matter. Higher-quality inputs cost more, and they last longer: a plasticiser that resists migration keeps a coating flexible for more seasons.

The Risk of Buying Cheap

As a buyer, poor UV stabilisation can’t easily be detected on a spec sheet before a grain cover is purchased or even within its first season. A cover made for milder climates, or with a cheap material, can look identical to a quality grain cover for its first season, before failing in later seasons, exposing the highly valuable grain underneath it. A failed cover means water damage, insect risk and failed fumigation.

That is why buying grain storage materials from a reputable supplier, with materials that have a strong track record in Australian conditions, is essential.